17-4PH, EN 1.4542, AISI 630 cold rolled stainless steel strip coil

FOB Reference Price:Get Latest Price
$1,000.00 - $10,000.00 / Metric Tons | 1 Metric Ton/Metric Tons (Min. Order)
Report Suspicious Activity
Overview
Quick Details
Grade:
600 Series
Standard:
AISI, ASTM, DIN, EN, JIS
Thickness:
0.1mm ~
Width:
500mm
Length:
in coil
Place of Origin:
Jiangsu, China (Mainland)
Brand Name:
changjiang
Model Number:
17-4PH, EN 1.4542,
Technique:
Cold Rolled
Application:
petrochemical, food processing
Certification:
SGS
material:
17-4PH, EN 1.4542, AISI 630, UNS S17400
Supply Ability
Supply Ability:
500 Metric Ton/Metric Tons per Month
Packaging & Delivery
Packaging Details
seaworthy.
Port
shanghai, china

17-4PH, EN 1.4542, AISI 630 cold rolled stainless steel strip coil

 

Steel 17-4 PH is a martensitic precipitation-hardening stainless steel that provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures
up to 600°F (316°C), good toughness in both base metal and welds, and shorttime, low-temperature heat treatments that minimize warpage and scaling. This versatile material is widely used in the aerospace, chemical, petrochemical, food processing, paper and general metalworking industries.

 

Designation

AISIENDIN
630, UNS S17400, 17-4PH1.4542X5CrNiCuNb17-4

 

COMPOSITION %
Carbon 0.07 max.
Manganese 1.00 max.
Phosphorus 0.040 max.
Sulfur 0.030 max.
Silicon 1.00 max.
Chromium 15.00 - 17.50
Nickel 3.00 - 5.00
Copper 3.00 - 5.00
Columbium plus Tantalum 0.15 - 0.45

 

Products supplied from the mill in Condition A, 17-4 PH Stainless Steel can be heat treated at a variety of
temperatures to develop a wide range of properties. Eight standard heat treatments have been developed.

 

 

 

Condition A
Solution Treated
1900°F ± 25°F
(1038°C ± 14°C)
Air cool below
90°F (32°C)

ConditionHeat to +/- 15ºF ( 8.4ºC )Time at Temperature, hourType of Cooling
H 900900°F (482°C)1Air
H 925925°F (496°C)4Air
H 10251025°F (551°C)4Air
H 10751075°F (580°C)4Air
H 11001100°F (593°C)4Air
H 11501150°F (621°C)4Air
H 1150 + 1150

1150°F (621°C)

1150°F (621°C)

4 followed by 4Air
H 1150-M

1400°F (760°C)

1150°F (621°C)

2 followed by 4Air

 

MECHANICAL PROPERTIES
Typical Mechanical Properties

PropertyAH 900H 925Condition H 1025H 1075H 1150H 1150-M
UTS, ksi ( Mpa )160 ( 1103 )210 ( 1448 )200 ( 1379 )185 ( 1276 )175 ( 1207 )160 ( 1103 )150 ( 1034 )
0.2%, YS, ksi ( Mpa )145 ( 1000 )200 ( 1379 )195 ( 1345 )170 ( 1172 )165 ( 1148 )150 ( 1034 )130 ( 896 )

Elongation, % in 2''

( 50.8mm )

5.07.08.08.08.011.012.0
Hardness, rockwellC35C45C43C38C37C35C33

 

AMS 5604 Sheet, Strip and Plate
ASTM A 693 Plate, Sheet and Strip